Leave it to us for vacuum devices and vacuum pumps!
Using a water-cooled copper mold for melting in an inert gas (Ar.He) atmosphere allows for extremely good melting without oxidation or nitriding of the sample, and there is no contamination from the crucible.
【Features】
○ It is one of the melting methods that is absolutely essential for metals that react with refractory crucibles.
○ The entire process from evacuation to melting is completed in just a few minutes, making it easy to operate even for those without experience.
○ Melting under reduced pressure above the stable arc region of 7×10^-3 Pa has a degassing effect.
○ The electrodes can be moved up, down, front, back, and sideways through a universal seal.
Therefore, sufficient stirring of the sample can be achieved, resulting in a uniform alloy.
○ Ignition is easy with the arc starter, and there is almost no pickup with W electrodes.
○ By changing the mold, samples of any size and shape can be obtained.
○ The use of a water-cooled jacket type chamber ensures that the chamber does not get hot even during continuous melting, making it safe.