Quality degradation due to grinding of the spring end face and heat generation, and points to note.
[Reproduction of Private Spring Preparatory School Lecture 42] Thin wire springs, thick wire springs! An explanation of the issues of end face grinding and shot peening for both.
Even for the same type of wire springs, when the wire diameter is thick and reaches 12 millimeters or more, the manufacturing process changes as follows: ■ Material: Annealed wire ■ Process: Coiling → Cutting → Hardening → Tempering → End face grinding → Setting In some cases, shot peening may be performed after end face grinding, similar to fine wire springs. Now, let's study the common issues of both fine wire springs and thick wire springs, specifically end face grinding and shot peening. *For detailed content of the article, please refer to the PDF. For more information, feel free to contact us.*