We will introduce a case that visualizes how the hardness distribution varies significantly with each nitriding treatment.
We will introduce a case study that tested three types of nitriding treatments on the same material. As a result, it was found that there are weak areas on the surface, and that strength and thickness vary significantly depending on the treatment. 【Case Overview】 ■Objective - To identify the strength (hardness) distribution in the depth direction from the surface of shallow surface-treated materials. ■Evaluation - Gas nitriding achieved the minimum erosion rate (maximum hardness) at a depth of 8µm, remained constant up to 12µm, and then gradually increased the erosion rate (hardness decreased) until reaching 20µm, where it stabilized. *For more details, please refer to the PDF document or feel free to contact us.
Inquire About This Product
basic information
For more details, please refer to the PDF document or feel free to contact us.
Price range
Delivery Time
Applications/Examples of results
For more details, please refer to the PDF document or feel free to contact us.
catalog(1)
Download All CatalogsCompany information
Amid the significant trend of paradigm shifts, through creativity-driven research and development, we aim to propose new surprises—values and technologies, as well as next-level efficiency and quality—to our society, spreading all these surprises to the world and creating a vast network of "monozukuri" (manufacturing) and "kotozukuri" (value creation). We aspire to expand a network of manufacturing that encompasses the world, starting from Nagaoka, a city representing Niigata, a region known for its industrial development.