List of Contract Services products
- classification:Contract Services
2476~2490 item / All 4764 items
We conduct various analyses primarily focused on polymers, plastics, and composite materials.
- Contract Analysis
In addition to the standard FT-IR functions, it allows for the qualitative analysis of small material portions, making it effective for foreign substance (contamination) analysis and troubleshooting.
- Contract Analysis
Measurement of the relative molecular weight and molecular weight distribution of polymers and oligomers.
- Contract Analysis
Analysis of RoHS and ELV regulated substances (elements). Accredited testing laboratory under ISO 17025.
- Contract Analysis
Attach strain gauges that are orthogonal to the center of the specimen, or uniaxial gauges at 0° and 90°, to measure longitudinal and transverse strain.
- Contract measurement
Measure the behavior changes during cooling [P (pressure) - V (volume) - T (temperature)] and use it as simulation data for flow analysis and mold design.
- Contract measurement
20mm vertical burning test (IEC 60695-11-10 Method B, ASTM D3801)
- Contract measurement
Horizontal combustion test (IEC 60695-11-10 Method A, ASTM D635)
- Contract measurement
Vertical Combustion Test for Thin Materials (ASTM D4804)
- Contract measurement
125mm vertical combustion test (IEC60695-11-20, ASTM D5048)
- Contract measurement
Horizontal combustion test of foamed materials (ISO 3582, JIS K6400-6, ASTM D4986)
- Contract measurement
The oil temperature is raised at a constant rate (120°C/h), and a specified bending stress is applied to the sample, with the temperature at which the specified deflection is reached being defined as ...
- Contract measurement
The temperature at which the penetration depth of a needle with a cross-sectional area of 1 mm² reaches 1 mm under a specified load, while the oil temperature is steadily increased in the oil, is refe...
- Contract measurement
It is represented as BPT when a φ5mm steel ball is pressed with a load of 20N for 1 hour in oil at the test temperature, resulting in a sample indentation depth of 0.209mm.
- Contract measurement
The temperature that causes destruction with a 50% probability during impact testing in low temperatures with methanol/dry ice is referred to as the embrittlement temperature.
- Contract measurement